Isakazwa Ingilazi yokushisa okushisa
Ingilazi isetshenziswe njengezinto zokubamba ukushisa okushisa okomlilo okweqile eminyakeni engamashumi amaningi ikakhulukazi ngenxa yokudluliswa kwayo okuphezulu kokukhanya nokuphila isikhathi eside. Yize ingilazi idlulisa amaphesenti aphezulu okukhanya kwelanga, iningi lalokho kukhanya lingena phakathi kokucwebezela ngendlela eqondisayo; kuncane kakhulu okusakazekile.
Ingilazi esetshenzisiwe ivame ukwenziwa ngokuphatha ingilazi enensimbi ephansi ukudala amaphethini asabalalisa ukukhanya. Uma kuqhathaniswa nengilazi ecacile, ingilazi esakazekile ingakwazi:
- Khulisa ukufana kwesimo sezulu esibamba ukushisa, ikakhulukazi izinga lokushisa nezimo zokukhanya
- Khulisa ukukhiqizwa kwezithelo (ngamaphesenti ama-5 kuye kwayi-10) wezilimo zikatamatisi nezikhukhamba eziphakeme
- Khulisa ukuqhakaza futhi unciphise isikhathi sokukhiqizwa kwezitshalo ezinamanzi njenge-chrysanthemum ne-anthurium.
Ingilazi esetshenzisiwe ihlukaniswe yaba:
Sula ingilazi enomusa kaMat
Ingilazi Ephansi Ye-Iron Matt Matt
Sula uMat Omnene
Ingilazi ye-Iron Prismatic ephansi
Ingilazi enephethini ephansi ye-Iron eyenziwe ngephethini le-mat ebusweni obunye kanye nephethini le-mat kobunye ubuso.Lokhu kuqinisekisa ukudluliswa kwamandla okuphezulu kakhulu kulo lonke i-spectrum yelanga.
Ingilazi ye-Low Iron Prismatic eyenziwe ngephethini le-mat ebusweni obunye nolunye uhlangothi lubushelelezi.
Omnene Glass uvumelana EN12150, Okwamanje, singenza Anti-reflection enamathela engilazini.
Imininingwane | Ukusabalalisa Ingilazi 75 Haze | Ukusabalalisa i-Glass 75 Haze ene-2 × AR |
Ubukhulu | 4mm ± 0.2mm / 5mm ± 0.3mm | 4mm ± 0.2mm / 5mm ± 0.3mm |
Ubude / Ububanzi Ukubekezelelana | ± 1.0mm | ± 1.0mm |
Ukubekezelelana Okudayelana | ± 3.0mm | ± 3.0mm |
Ubukhulu | Ubukhulu. 2500mm X 1600mm | Ubukhulu. 2500mm X 1600mm |
Iphethini | Nashiji | Nashiji |
Qeda-Qeda | C-onqenqemeni | C-onqenqemeni |
Inkungu (± 5%) | 75% | 75% |
I-Hortiscatter (± 5%) | 51% | 50% |
I-LT ejwayelekile (± 1%) | 91.50% | 97.50% |
I-Hemispherical LT (± 1%) | 79.50% | 85.50% |
Okuqukethwe kwe-Iron | Fe2 + -120 ngomzuzu | Fe2 + -120 ngomzuzu |
Umnsalo Wendawo | ≤2 ‰ (Max 0.6mm ngaphezu kwebanga elingu-300mm) | ≤2 ‰ (Max 0.6mm ngaphezu kwebanga elingu-300mm) |
Sekukonke umnsalo | ≤3 ‰ (Max 3mm ngaphezu kwebanga elingu-1000mm) | ≤3 ‰ (Max 3mm ngaphezu kwebanga elingu-1000mm) |
Amandla Mechanical | > 120N / mm2 | > 120N / mm2 |
Ukuphuka okuzenzakalelayo | <300 ppm | <300 ppm |
Isimo Sezingcezu | Ubuncane. Izinhlayiya 60 ngaphakathi 50mm × 50mm; Ubude bezinhlayiya ezinde kakhulu <75mm |
Ubuncane. Izinhlayiya 60 ngaphakathi 50mm × 50mm; Ubude bezinhlayiya ezinde kakhulu <75mm |
Ukumelana Okushisayo | Kuze kufike ku-250 ° Celsius | Kuze kufike ku-250 ° Celsius |
Ukuboniswa Komkhiqizo
![4mm-Clear-Mistlite-Nashji-Matt-Diffused-Glass-for-Greenhouse](http://www.lydglass.com/uploads/962ba975-300x300.jpg)
![5453272e3f6c6a02cb59de35cbe938c3](http://www.lydglass.com/uploads/61840fe4-300x300.jpg)
![201508282208112_副本](http://www.lydglass.com/uploads/9f62fadf-300x300.jpg)